Spesifikasi
| Ciri | XS-FR-8800 | XS-FR-8801 | XS-FR-8802 | XS-FR-8802LC |
| Keputihan | ≥88 | ≥88 | ≥88 | ≥88 |
| Kandungan Bromin % | 26 ± 3 | 6 ± 3 | 0.1 | 20 ± 3 |
| H ₂ O kandungan % | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 |
| Ketumpatan relatif | 1.5 ~ 1.7 | 1.1 ~ 1.2 | 1.5 ~ 1.7 | 1.5 ~ 1.7 |
| Ketumpatan pukal | ~ 0.8 | ~ 0.6 | ~ 0.8 | ~ 0.6 |
| Rintangan suhu | ★★★ | ★★★★ | ★★★★★ | ★★★★★ |
| Pemendakan tahan | ★★★ | ★★★★★ | ★★★★ | ★★★★ |
| Mobiliti | ★★★ | ★★★ | ★★★★★ | ★★★ |
| Suhu penyemperitan | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ |
| Cahaya wayar | Gwit 750 ℃ & gwfi 850 ℃ | |||
| Kebolehgunaan | Bukan Fil | Mengisi/diperkuat | Temp.Resistance Halogen rendah | Temp.Resistance |
| Dos % | XS-FR-8800 | XS-FR-8801 | XS-FR-8802 | XS-FR-8802LC | |||||||||
| Padding % | 0 | 15 | 30 | 0 | 15 | 30 | 0 | 15 | 30 | 0 | 15 | 30 | |
| Co-PP | 0.8mm V-2 | 2.5 | --- | --- | 2.5 | --- | --- | 2.5 | --- | --- | 2.5 | --- | --- |
| 1.6mm V-2 | 3 | --- | --- | 3 | --- | --- | 3 | --- | --- | 3 | --- | --- | |
| 3.2mm V-2 | 3 | --- | --- | 3 | --- | --- | 3 | --- | --- | 3 | --- | --- | |
| 0.8mm V-2 | 1 | --- | --- | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | |
| Ho-PP | 1.6mm V-2 | 1 | --- | --- | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 |
| 3.2mm V-2 | 1 | --- | --- | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | |
| Catatan | Sesetengah pengisi akan menjejaskan kebencian api (seperti kalsium karbonat, magnesium karbonat, dan lain -lain) | ||||||||||||
| Ciri | XS-FR-8803 | XS-FR-8805 | XS-FR-8810 | XS-FR-8820 |
| Keputihan | ≥92 | ≥88 | ≥88 | ≥88 |
| Kandungan Bromin% | 10 ± 3 | ≤2 | 0.1 | 20 ± 3 |
| H ₂ O kandungan % | ≤0.5 | ≤0.5 | ≤1.0 | ≤1.0 |
| Ketumpatan relatif | 1.6 ~ 1.8 | 1.1 ~ 1.2 | 1.5 ~ 1.7 | 1.5 ~ 1.7 |
| Ketumpatan pukal | ~ 0.8 | ~ 0.5 | ~ 0.8 | ~ 0.6 |
| Rintangan suhu | ★★★ | ★★★ | ★★★★★ | ★★★★★ |
| Pemendakan tahan | ★★★ | ★★★ | ★★★★ | ★★★★ |
| Mobiliti | ★★★ | ★★★ | ★★★★★ | ★★★ |
| Suhu penyemperitan | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ |
| Glow wire | GWFI 800 ℃ | GWIT750 ℃/GWFI850 ℃ | ||
| Yang lain | Pengisian kecil | Pengisian kecil | Temp.Resistance Halogen rendah | Temp.Resistance |
| Dos % | XS-FR-8803 | XS-FR-8805 | XS-FR-8810 | XS-FR-8820 | |||||||||
| Padding % | 0 | 5 | 30 | 0 | 5 | 30 | 0 | 15 | 30 | 0 | 15 | 30 | |
| Co-PP | 0.8mm V-2 | 2.5 | 3 | --- | 2.5 | 3 | --- | 3 | 3 | --- | 3 | 10 | --- |
| 1.6mm V-2 | 3 | 3.5 | --- | 3 | 3.5 | --- | 3.5 | 3.5 | --- | 3.5 | 10 | --- | |
| 3.2mm V-2 | 3 | 3.5 | --- | 3 | 3.5 | --- | 3.5 | 3.5 | --- | 3.5 | 10 | --- | |
| 0.8mm V-Z | 0.8 | 1 | --- | 0.8 | 1 | --- | 1 | 1 | --- | 1 | 6 | --- | |
| Ho-PP | 1.6mm V-2 | 0.9 | 1.2 | --- | 0.9 | 1.2 | --- | 1 | 1.2 | --- | 1 | 6 | --- |
| 3.2mm V-2 | 1 | 1.3 | --- | 1 | 1.3 | --- | 1 | 1.3 | --- | 1 | 6 | --- | |
| Catatan | Sesetengah pengisi akan menjejaskan kebencian api (seperti kalsium karbonat, magnesium karbonat, dan lain -lain) Disyorkan untuk menambah barium sulfat, serbuk mika, manik kaca, dan lain -lain. Serbuk talc harus tinggi kandungan silikon. Gabungan skru ricih yang kuat tidak disyorkan untuk skru ricih; Tidak ada vakum atau vakum rendah dalam proses penyemperitan. | ||||||||||||
Kemudahan pembuatan di xusen
Dengan dua pangkalan pengeluaran yang terletak di Jiashan, Zhejiang, dan Juancheng, Shandong, kami kini mencapai kapasiti pengeluaran tahunan sebanyak 12,000 tan, yang terus berkembang. Kami bangga dengan Makmal Penyelidikan Saintifik Tahap Zhejiang kami. Kami mempunyai bengkel dan gudang pengeluaran kami sendiri, dilengkapi dengan peralatan pemeriksaan dan pemeriksaan kualiti yang lengkap.
Mengapa Poliamida Standard Terbakar — dan Perkara yang Selesaikan oleh Format Masterbatch Poliamida - dikenali secara meluas sebagai nilon - adalah salah satu plastik kejuruteraan yang paling po...
Baca lebih lanjutAmmonium polifosfat (APP) ialah salah satu kalis api bebas halogen yang paling banyak digunakan di dunia, dan untuk alasan yang baik. Ia menggabungkan kandungan fosforus dan nitrogen yang tinggi da...
Baca lebih lanjutKalis api telah menjadi bahagian standard pembuatan polimer dan kabel selama beberapa dekad. Bagi kebanyakan sejarah itu, kimia dominan bergantung pada halogen—sebatian bromin dan klorin yang sanga...
Baca lebih lanjutMelamin Sianurat (MCA) adalah kalis api bebas halogen yang dibentuk oleh gabungan equimolar melamin dan asid sianurik. Hasilnya ialah serbuk putih kristal yang stabil yang telah menjadi salah...
Baca lebih lanjut